IEEE-1275580 (pdf) Ceramic-based Multisite Electrode array for Chronic Single-Neuron Recording

  • Their substrate is polished to 35-50um thick
  • patterned using standard lift-off lithographic techniques
  • four electrodes per shank
  • The ceramic is considerably stiffer than silicon (table) -- 372 Gpa vs. 190 Gpa.